Skip to main content

Jak vypočítat Hall Petch

Co je Hall Petch?

Hall-Petch strengthening: yield strength = σ₀ + k·d^(-1/2), where d is grain diameter; primary strengthening mechanism.

Průvodce krok za krokem

  1. 1Input material constants σ₀ and k
  2. 2Vary grain size
  3. 3Calculate predicted yield strength

Worked Examples

Vstup
Steel: σ₀ = 50 MPa, k = 0.8 MPa√mm
Výsledek
1mm grains → 50.8 MPa, 0.01mm → 80 MPa strength increase

Common Mistakes to Avoid

  • Using wrong units for grain size
  • Applying beyond material's valid range

Frequently Asked Questions

Is Hall-Petch always linear?

Approximately yes; breaks down at very small grain sizes (<100 nm).

Jste připraveni počítat? Vyzkoušejte bezplatnou kalkulačku Hall Petch

Zkuste to sami →

Nastavení