Hall-Petch strengthening: yield strength = σ₀ + k·d^(-1/2), where d is grain diameter; primary strengthening mechanism.
Przewodnik krok po kroku
- 1Input material constants σ₀ and k
- 2Vary grain size
- 3Calculate predicted yield strength
Rozwiązane przykłady
Wejście
Steel: σ₀ = 50 MPa, k = 0.8 MPa√mm
Wynik
1mm grains → 50.8 MPa, 0.01mm → 80 MPa strength increase
Częste błędy do unikania
- ✕Using wrong units for grain size
- ✕Applying beyond material's valid range
Często zadawane pytania
Is Hall-Petch always linear?
Approximately yes; breaks down at very small grain sizes (<100 nm).
Gotowy do obliczeń? Wypróbuj darmowy kalkulator Hall Petch