Galvanic corrosion occurs when dissimilar metals contact in electrolyte; more active metal (anode) corrodes preferentially.
Step-by-Step na Gabay
- 1Input two metals and galvanic series position
- 2Calculate galvanic potential
- 3Determine which metal corrodes and rate
Mga Nalutas na Halimbawa
Input
Zinc (anode) + steel (cathode) in seawater
Resulta
Zinc sacrificially corrodes, protecting steel (intentional use)
Mga Karaniwang Mali na Dapat Iwasan
- ✕Assuming only one metal corrodes (wrong)
- ✕Not understanding sacrificial anode concept
Mga madalas itanong
How do you prevent galvanic corrosion?
Use same metal, isolate with non-conductive gasket, or apply protective coating.